Highly Concentrated Graphene Oxide (2 wt% Concentration)

Call for Price

Highly Concentrated Graphene Oxide (2 wt% Concentration)

Our Highly Concentrated Graphene Oxide allows the preparation of custom dispersions of different concentrations by just adding water and sonicating for 30 minutes.

PROPERTIES

  • Form: Slurry
  • Particle Size:
    • – D90 29 – 33 μm
    • – D50 14 – 17 μm
    • – D10 6 – 7 μm
  • Color: Dark brown
  • Odor: Odorless
  • Dispersibility: Polar solvents
  • Solvent: Water
  • pH: 1,8 – 2
  • Concentration: 2 wt%
  • Monolayer content (measured in 0.05 wt%): >95%

ELEMENTAL ANALYSIS

  • Carbon: 49 – 56%
  • Hydrogen: 1 – 2%
  • Nitrogen: 0 – 1%
  • Sulfur: 2 – 3%
  • Oxygen: 41 – 50%

 