Highly Concentrated Graphene Oxide Dispersion in Water

Concentration: 5g/L, 5 g per bottle

Composition: Carbon (≥ 46%), Oxygen (≤ 46%

Flake size: 0.5-5 microns

Thickness: 1 atomic layer – at least 60%.

Color:Brown

Available volume- 175 ml, 1000 ml